Products

    FCS 1.2083 Tool Steel
    1.2083 steel is suitable for die casting of steel, die and pressure tools and light non-ferrous metal alloys that are easily affected by corrosive plastic and polymer tools and inserts.
    1.2080 Tool Steel
    1.2080 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
    D2 Tool Steel | 1.2379 | X155CrVMo12-1 | SKD11
    As a benchmark for high carbon and high chromium cold work die steel, D2 steel's core highlight lies in the precise ratio of 12% chromium content and 1.5% carbon to form a large number of hard carbides. It maintains an ultra-high hardness of 60-62HRC while also having better wear resistance than ordinary tool steel (5-8 times that of ordinary steel). After appropriate heat treatment, D2 steel can significantly improve its anti cracking performance, especially suitable for high-strength wear scenarios such as precision punching dies and shear cutting tools. D2 steel, known as "semi stainless steel", also forms a passive film on its surface to delay corrosion, becoming a classic choice for balancing performance and cost in the industrial field.
    1.2363 Steel
    1.2363 steel has excellent wear resistance and compressive strength, while maintaining good toughness, making it particularly suitable for manufacturing high-precision cold work molds.
    FCS 1.2316 Tool Steel
    1.2316 is a kind of pre hardened and tempered plastic tool steel. Excellent corrosion resistance, excellent wear resistance and toughness, good thermal fatigue resistance, uniform material hardness and superior polishing performance. 1.2316 tool steel is especially suitable for thermoplastic corrosive plastics, transparent and mirror products and molds.
    AISI H11 Tool Steel | 1.2343 | X37CrMoV5-1 | SKD6 | BH11
    As an air-cooled hardening type hot work die steel, H11 steel has excellent high-temperature strength and toughness. Its chromium molybdenum vanadium alloy system endows it with excellent heat fatigue resistance and wear resistance. H11 steel maintains high hardness under 500-600 ℃ working conditions, while also having good cutting and heat treatment stability, making it particularly suitable for the manufacturing of aluminum/magnesium alloy die-casting molds and hot forging dies.
    FCS 1.2714 Hot Work Tool Steel
    1.2714 steel material exhibits excellent thermal fatigue resistance and corrosion resistance in die casting applications, and its microstructural stability enables it to maintain performance under long-term thermal cycling conditions. Compared to similar materials, 1.2714 steel has better resistance to softening and processing adaptability, making it the preferred material for high-end hot work molds.
    FCS O1 Tool Steel | 1.2510 | 100MnCrW4 | SKS3
    O1 mold steel is widely used. O1 steel has good processability, good wear resistance, stable O1 heat treatment performance, small dimensional deformation, but weak toughness and corrosion resistance. It is commonly used in blanking die, punching die, punching die, punching die, etc.
    S7 Tool Steel
    S7 steel is a kind of air or Oil hardened tool steel with high impact toughness. The combination of strength and high toughness makes it a candidate for various tool applications. S7 tool steel is often used for cold working tools that need to resist high impact and impact loads, such as shear blades, forging dies, clamping dies, chisels and punches.
    440C Plastic Mould Steel
    440C steel is a high carbon, high chromium martensitic stainless steel known for its high hardness, wear resistance, and corrosion resistance. It is widely used in fields such as cutting tools, bearings, and medical devices.

Products

Featured products

  • H11 Tool Steel
    H11 Tool Steel
    H11 steel combines high hardness and toughness, and exhibits outstanding performance under extreme working conditions. H11 steel has excellent hardenability and can be hardened by air cooling, greatly reducing the risk of mold heat treatment deformation and cracking; H11 steel has stable thermal strength and oxidation resistance under medium temperature environment, and can maintain good mechanical properties within 600 ℃. It has strong resistance to cold and hot fatigue, and is not easy to crack under frequent cold and hot cycles. H11 steel has excellent resistance to low melting point alloys such as aluminum and magnesium.
    More
  • 1.2581 Hot Work Tool Steel
    1.2581 Hot Work Tool Steel
    1.2581 hot work mold steel is a commonly used die-casting mold steel. 1.2581 steel has high strength and hardness, good resistance to cold and hot fatigue, and good hardenability.
    More
  • 1.2343 Tool Steel
    1.2343 Tool Steel
    1.2343 steel is a hot work die steel with high toughness and wear resistance. Its core advantages lie in excellent heat fatigue resistance and high-temperature strength. 1.2343 steel is very suitable for high-temperature working environments such as die-casting and forging.
    More
  • D2 Tool Steel
    D2 Tool Steel
    D2 steel is suitable for making all kinds of cold stamping dies with large cross-section and complex shape, as well as cold cutting scissors and thread taking plates; Cold extrusion forming, trimming die, etc
    More