High Speed Steel

    M42 high-speed steel
    M42 high-speed steel is a high-quality cobalt high-speed steel. Its chemical composition is designed specifically for high hardness and excellent thermal hardness. These characteristics make M42 high-speed steel the best choice for processing high-strength and pre hardened steels, high hardness alloys, and difficult to machine non-ferrous metal superalloys used in the aerospace, petroleum, and power generation industries. The cutting tool made of M42 high-speed steel can cut iron-based high-temperature alloys, cast high-temperature alloys, titanium alloys, and ultra-high strength steels. Due to its excellent grindability, it can be used to manufacture various high-precision and complex cutting tools.
    1.3355 High Speed Steel
    1.3355 high speed steel has good ductility and is used for roughing and finishing tools with medium strength parameters. 1.3355 high speed steel can be used to produce turning tools, chisel tools, turning and planer, milling cutter, drill bit, thread tool, saw blade, planer, small circular saw, reamer, tap and screw cutter processed on automatic machinery.
    M2 HIGH SPEED STEEL
    M2 steel is a tungsten molybdenum high-speed steel with good hardness and wear resistance. Mainly used for manufacturing cutting tools for difficult to cut materials. M2 high-speed steel is suitable for molds that can withstand vibration and impact loads: deep drawing molds, stamping molds, metal cutting blades, cold heading and extrusion tools.

    Products

    Featured products

    • M42 high-speed steel
      M42 high-speed steel
      M42 high-speed steel is a high-quality cobalt high-speed steel. Its chemical composition is designed specifically for high hardness and excellent thermal hardness. These characteristics make M42 high-speed steel the best choice for processing high-strength and pre hardened steels, high hardness alloys, and difficult to machine non-ferrous metal superalloys used in the aerospace, petroleum, and power generation industries. The cutting tool made of M42 high-speed steel can cut iron-based high-temperature alloys, cast high-temperature alloys, titanium alloys, and ultra-high strength steels. Due to its excellent grindability, it can be used to manufacture various high-precision and complex cutting tools.
      More
    • 1.3355 High Speed Steel
      1.3355 High Speed Steel
      1.3355 high speed steel has good ductility and is used for roughing and finishing tools with medium strength parameters. 1.3355 high speed steel can be used to produce turning tools, chisel tools, turning and planer, milling cutter, drill bit, thread tool, saw blade, planer, small circular saw, reamer, tap and screw cutter processed on automatic machinery.
      More
    • M2 HIGH SPEED STEEL
      M2 HIGH SPEED STEEL
      M2 steel is a tungsten molybdenum high-speed steel with good hardness and wear resistance. Mainly used for manufacturing cutting tools for difficult to cut materials. M2 high-speed steel is suitable for molds that can withstand vibration and impact loads: deep drawing molds, stamping molds, metal cutting blades, cold heading and extrusion tools.
      More