    1.2085 Steel
    1.2085 steel is a pre hardened martensitic stainless steel with excellent corrosion resistance and good mechanical processing performance. It is particularly suitable for plastic molds and cold work molds that require rust prevention, especially for processing corrosive plastic materials.