D6|1.2436|Cr12W

    FCS D6 Tool Steel
    As a representative of high-end cold work die steel, D6 steel's core highlight lies in achieving excellent balance between wear resistance and crack resistance through high carbon and high chromium alloy design, and significantly improving dimensional stability through deep cryogenic treatment technology; D6 steel exhibits excellent deformation resistance and durability in harsh working conditions such as silicon steel sheet punching and precision processing of high-strength steel plates, while also possessing good corrosion resistance, making it an ideal choice for high-precision and high load mold manufacturing.
    Cr12W Tool Steel
    The highlight of Cr12W steel as a high-end cold work die steel lies in its excellent wear resistance (62-64HRC) and perfect balance of toughness. Cr12W steel significantly improves its red hardness by adding 1% tungsten element, ensuring stable performance of the die at 300 ℃; The optimized carbide distribution of Cr12W steel gives it three times the service life of ordinary mold steel, making it particularly suitable for precision electronic component stamping and automotive part forming.
    1.2436 Tool Steel
    1.2436 steel is suitable for medium load stamping die, stamping stainless steel, copper, silicon, aluminum, etc.
    X210CrW12 Steel
    X210CrW12 steel is a high carbon, high chromium tungsten alloy tool steel, belonging to cold work die steel. X210CrW12 steel is renowned for its excellent wear resistance, high hardness, and good dimensional stability, making it particularly suitable for manufacturing high-precision, high wear resistant cold work molds and tools.

    Products

    Featured products

    • FCS D6 Tool Steel
      FCS D6 Tool Steel
      As a representative of high-end cold work die steel, D6 steel's core highlight lies in achieving excellent balance between wear resistance and crack resistance through high carbon and high chromium alloy design, and significantly improving dimensional stability through deep cryogenic treatment technology; D6 steel exhibits excellent deformation resistance and durability in harsh working conditions such as silicon steel sheet punching and precision processing of high-strength steel plates, while also possessing good corrosion resistance, making it an ideal choice for high-precision and high load mold manufacturing.
      More
    • Cr12W Tool Steel
      Cr12W Tool Steel
      The highlight of Cr12W steel as a high-end cold work die steel lies in its excellent wear resistance (62-64HRC) and perfect balance of toughness. Cr12W steel significantly improves its red hardness by adding 1% tungsten element, ensuring stable performance of the die at 300 ℃; The optimized carbide distribution of Cr12W steel gives it three times the service life of ordinary mold steel, making it particularly suitable for precision electronic component stamping and automotive part forming.
      More
    • 1.2436 Tool Steel
      1.2436 Tool Steel
      1.2436 steel is suitable for medium load stamping die, stamping stainless steel, copper, silicon, aluminum, etc.
      More
    • X210CrW12 Steel
      X210CrW12 Steel
      X210CrW12 steel is a high carbon, high chromium tungsten alloy tool steel, belonging to cold work die steel. X210CrW12 steel is renowned for its excellent wear resistance, high hardness, and good dimensional stability, making it particularly suitable for manufacturing high-precision, high wear resistant cold work molds and tools.
      More