L6 steel is a multi-purpose Oil hardened, heat-resistant and wear-resistant forged steel tool steel with very good toughness.
L6 tool steel is suitable for tools, molds and mechanical parts. They need a good combination of hardness and toughness. The relatively high nickel content makes the alloy have greater impact toughness than other ordinary oil hardening grades.