Fcs

    FCS 9CrWMn Tool Steel
    9CrWMn steel is a cold work die steel with high hardness, excellent wear resistance, and small quenching deformation, known as "micro deformation steel". 9CrWMn steel is particularly suitable for manufacturing high-precision molds with small cross-sections and complex shapes, such as cold stamping dies, gauges, etc.
    NAK80 plastic mold steel | P21 | 10Ni3MnCuAl Mold Steel
    NAK80 steel is a pre hardened plastic mold steel with high hardness (HRC37-43), excellent mirror polishing properties, and good electrical discharge machining performance. It is suitable for high-precision injection molds, optical product molds, and other scenarios. The pre hardening characteristics of NAK80 steel can reduce the risk of heat treatment deformation, while also having good weldability and corrosion resistance.
    FCS 4Cr13 Plastic Mould Steel
    The biggest advantage of 4Cr13 steel is its high hardness, good wear resistance, and good corrosion resistance. 4Cr13 steel is particularly suitable for manufacturing cutting tools, medical devices, molds, and durable parts that require rust prevention.
    FCS 9Cr18Mo Plastic Mould Steel
    9Cr18Mo steel, as a high carbon and high chromium martensitic stainless steel, has shown significant value in multiple industrial fields due to its excellent hardness and corrosion resistance, especially in providing the wear resistance required for high-precision cutting tools in tool manufacturing. The addition of molybdenum significantly enhances the corrosion resistance of the material, ensuring its stability in harsh environments. The 9Cr18Mo steel grade can achieve a balance of strength and toughness through optimized heat treatment processes, and is widely used in core components such as bearings, precision molds, and chemical equipment.
    AISI 420SS | DIN 1.2083 | JIS SUS420J2
    1.2083 steel is a high chromium stainless steel with excellent corrosion resistance, high hardness, and wear resistance, as well as good polishing performance. 1.2083 steel is commonly used to manufacture high demand plastic molds and optical components.
    FCS 1.2358 tool steel
    1.2358 mold steel has excellent wear resistance and good processing performance, and is widely used in industrial fields such as automotive parts stamping molds, injection mold inserts, precision shear blades, and hot forging molds below 600 ℃ (requiring coating). 1.2358 steel is particularly suitable for high-precision and high load mold manufacturing requirements.
    FCS 1.2345 steel
    1.2345 steel, as a material for die-casting molds, is suitable for manufacturing high-temperature components of aluminum/magnesium alloys and can extend the life of zinc/copper alloy die-casting molds through surface strengthening processes. In the field of hot processing, its high temperature stability supports the long-term use of titanium alloy extrusion molds and automotive forging hot forging dies. In the application of plastic molds, 1.2345 steel has the ability to withstand high temperature engineering plastic injection molding and optical grade surface treatment, while exhibiting better wear resistance than traditional materials in precision stamping and powder metallurgy fields.
    FCS 1.2746 Tool Steel
    1.2746 steel exhibits excellent versatility in both cold and hot working applications. As a high-quality tool steel, it performs well in cold working molds (stamping, stretching, cold heading) for automotive and electronic manufacturing due to its excellent wear resistance and deformation resistance under high loads. Meanwhile, the excellent high-temperature stability and thermal fatigue resistance of 1.2746 steel make it an ideal choice for hot forging and die-casting molds in the aerospace and home appliance industries, significantly extending the service life of the molds while maintaining accuracy under extreme conditions (up to 400 ° C). This dual capability stems from its optimized alloy composition, which has balanced nickel chromium molybdenum vanadium elements.

Products

Featured products

  • FCS D6 Tool Steel
    FCS D6 Tool Steel
    As a representative of high-end cold work die steel, D6 steel's core highlight lies in achieving excellent balance between wear resistance and crack resistance through high carbon and high chromium alloy design, and significantly improving dimensional stability through deep cryogenic treatment technology; D6 steel exhibits excellent deformation resistance and durability in harsh working conditions such as silicon steel sheet punching and precision processing of high-strength steel plates, while also possessing good corrosion resistance, making it an ideal choice for high-precision and high load mold manufacturing.
    More
  • FCS 3Cr17NiMo-MOD STEEL
    FCS 3Cr17NiMo-MOD STEEL
    3Cr17NiMo MOD STEEl is a kind of pre hardened and tempered plastic tool steel. Excellent corrosion resistance, excellent wear resistance and toughness, good thermal fatigue resistance, uniform material hardness and superior polishing performance. 3Cr17NiMo MOD STEEL is especially suitable for thermoplastic corrosive plastics, transparent and mirror products and molds.
    More
  • FCS 1.2316 Tool Steel
    FCS 1.2316 Tool Steel
    1.2316 is a kind of pre hardened and tempered plastic tool steel. Excellent corrosion resistance, excellent wear resistance and toughness, good thermal fatigue resistance, uniform material hardness and superior polishing performance. 1.2316 tool steel is especially suitable for thermoplastic corrosive plastics, transparent and mirror products and molds.
    More
  • FCS 1.2767 Tool Steel
    FCS 1.2767 Tool Steel
    1.2767 steel has good wear resistance, high toughness, high hardness, high compressive strength, excellent dimensional stability, excellent corrosion resistance, good polishing and pin cutting performance, and easy to achieve mirror effect. Good hardenability, air cooling hardening, good machining performance.
    More

Contact us

40px

40px

40px

40px

40px

80px

80px

80px

Get the latest price? We will reply as soon as possible (within 12 hours)

40px

40px

40px

40px