NAK80 plastic mold steel | P21 | 10Ni3MnCuAl Mold Steel
- fucheng steel
- China
- 1 Month
- 2000 Tons/Month
NAK80 PLASTIC MOLD STEEL
| Brand | FCS |
| Smelting and Manufacture Method: | LF+VD+Forged |
| Delivery Condition: | Annealed |
| Delivery hardness: | ≤43 HRC |
| UT Test Standard: | Sep 1921-84 Class3 D/d,E/e |


NAK80 STEEL GRADE COMPARISON AND CHEMICAL COMPOSITION COMPARISON
| Standard/Steel Grade | Chemical Composition(%) | ||||||||
| C | Si | Mn | Cr | Mo | W | Al | Cu | ||
| JIS | NAK80 | 0.15 | 0.30 | 0.15 | 0.30 | 0.30 | 0.30 | 1.10 | 1.00 |
APPLICATION
NAK80 plastic tool steel is suitable for high-efficiency blanking die, punching die and embossing die, all kinds of scissors, inlaid blade, woodworking blade, thread rolling die and wear-resistant slider, cold heading die, thermosetting resin forming die, deep drawing forming die and cold extrusion die.
Characteristics of NAK80 plastic mold steel:
1. High hardness and wear resistance
The factory hardness of NAK80 plastic mold steel is about HRC 37-43, and it can be used directly without heat treatment.
Suitable for manufacturing high-precision wear-resistant molds.
2. Excellent polishing performance
NAK80 plastic mold steel has a uniform and delicate structure, and can achieve a mirror effect after polishing, making it suitable for molds with high surface requirements.
3. Good processing performance
The pre hardened state of NAK80 plastic mold steel is still easy to cut, reducing processing difficulty and cost.
4. Corrosion resistance
NAK80 plastic mold steel has certain corrosion resistance and is suitable for humid or corrosive environments.
5. Dimensional stability
NAK80 plastic mold steel has minimal deformation after heat treatment and is suitable for high-precision mold manufacturing.
6. Solderability
NAK80 plastic mold steel has good welding performance and is easy to maintain and modify molds.
7. Material stability
NAK80 steel, as a pre hardened steel grade, reaches a hardness of HRC 37-43 from the factory. The microstructure is treated with special aging to form Ni3Al precipitates, ensuring that the hardness fluctuation before and after processing is ≤ 2 HRC. This characteristic completely avoids the risk of quenching deformation in traditional mold steel, and is particularly suitable for the rapid production of precision molds.
8. Surface finishing capability
NAK80 steel adopts ESR electroslag remelting process to control the content of non-metallic inclusions<0.001%, combined with ultrafine grain structure (ASTM grade 12), which can achieve mirror level polishing (Ra ≤ 0.012 μ m). Actual testing shows that its polishing efficiency is 40% higher than that of S136 steel, meeting the requirements of optical grade transparent parts molds.
9. Chemical compatibility
The unique copper nickel alloy system (Cu 1.0%/Ni 3.0%) of NAK80 steel endows it with excellent corrosion resistance. When forming halogen containing flame retardants (such as PVC), the corrosion rate is only 1/5 of P20 steel. Simultaneously possessing the ability to resist acid gas erosion, extending the maintenance cycle of the mold.
10. Thermal processing adaptability
During the discharge machining of NAK80 steel, only a white layer of ≤ 15 μ m is produced on the surface, and no secondary polishing is required. The welding repair performance is outstanding, and after 500 ℃ × 5h aging, the hardness recovery rate of the heat affected zone reaches 97%, significantly reducing the repair cost of complex molds.