AISI 420SS | DIN 1.2083 | JIS SUS420J2

1.2083 steel is a high chromium stainless steel with excellent corrosion resistance, high hardness, and wear resistance, as well as good polishing performance. 1.2083 steel is commonly used to manufacture high demand plastic molds and optical components.
  • fucheng steel
  • China
  • 1 Month
  • 2000 Tons/Month

1.2083 PLASTIC MOLD STEEL

Brand
FCS
Smelting and Manufacture Method:LF+VD+Forged
Delivery Condition:Annealed
Delivery hardness:≤225 HBS
UT Test Standard: Sep 1921-84 Class3 D/d,E/e

1.2083 plastic mold steel

420SS

1.2083 STEEL GRADE COMPARISON AND CHEMICAL COMPOSITION COMPARISON

Standard/Steel GradeChemical Composition(%)
CSiMnCr
DIN/W-Nr.X42Cr13/1.20830.38~0.45≤1.00≤1.0012.5~13.5
ASTM420SS0.30~0.40≤1.00≤1.2512.0~14.0
JISSUS420J20.26~0.40≤1.00≤1.0012.0~14.0


APPLICATION

1.2083 mold steel is suitable for electric etching operation, acid plastics and dies requiring good polishing. It is mainly used in the production of PVC molds, wear resistance and filler molds, including thermosetting plastic molds and long-life molds, such as molds for disposable tableware, production of optical product components, such as cameras, solar lenses, medical containers, etc.


1.2083 STEEL CHARACTERISTICS


1.2083 plastic mold steel is a special purpose steel mainly used for manufacturing plastic injection molds. Due to its excellent performance characteristics, 1.2083 plastic mold steel has a wide range of applications in the field of plastic mold manufacturing. The following are the main characteristics of 1.2083 plastic mold steel:


Good wear resistance: 1.2083 steel has high hardness and can maintain good wear resistance during long-term use. This makes the mold less prone to wear and tear during use, extending its service life.


High fatigue resistance: 1.2083 steel has good fatigue resistance and can maintain good working condition under high-strength and high-frequency usage conditions. This makes the mold less prone to fatigue fracture during use, improving the reliability of the mold.


Good heat treatment performance: 1.2083 steel has good heat treatment performance, and the hardness and toughness of the steel can be adjusted through the heat treatment process to meet the usage requirements under different working conditions. This enables the mold to maintain good dimensional stability and surface smoothness during use.


Good polishing performance: 1.2083 steel has good polishing performance, which can achieve high surface smoothness through polishing process and improve the molding effect of the mold.


Good welding performance: 1.2083 steel has good welding performance and can connect multiple parts together through welding processes, meeting the manufacturing requirements of complex shaped molds.


Good corrosion resistance: 1.2083 steel has good corrosion resistance and can maintain a good service life in various corrosive environments. This makes the mold less susceptible to corrosion during use, improving its service life.


Good machining performance: 1.2083 steel has good machining performance and can achieve high dimensional accuracy and surface smoothness through cutting, grinding and other processing techniques. This enables the mold to maintain a good molding effect during use.


Environmental friendliness: 1.2083 plastic mold steel has a relatively small impact on the environment during the production process and meets environmental protection requirements. This makes 1.2083 plastic mold steel have great potential for application in the field of green manufacturing.


Good market demand: With the widespread application of plastic products in various fields, the demand for plastic molds is increasing. With its excellent performance characteristics, 1.2083 plastic mold steel meets the market demand for high-quality and high-performance plastic molds, and has a high market demand.


SUS420J2

1.2083 plastic mold steel

420SS

SUS420J2

1.2083 plastic mold steel


40px

80px

80px

80px

Get the latest price? We will reply as soon as possible (within 12 hours)

40px

40px

40px

40px