Cold Work Tool Steel

    O2 Tool Steel
    O2 steel, as a typical oil quenched die steel, exhibits superior hardness and wear resistance as its core characteristics. After standardized heat treatment, the hardness of O2 steel remains stable in the range of 58-62 HRC, with high carbon content (1.55-1.70%) forming uniform carbides with chromium elements, significantly improving the material's wear resistance, especially suitable for high load stamping scenarios. O2 steel is widely used in the manufacturing of small punching dies, gauges, and machine tool screws.
    FCS SKD1 Tool Steel
    SKD1 steel, as a classic cold work mold material, has achieved high hardness performance of 58-61HRC through optimized alloy ratio and heat treatment process, making it particularly suitable for cold stamping molds and scissor blades that require extreme wear resistance. SKD1 steel has excellent heat treatment stability. After quenching, low-temperature tempering can eliminate stress and minimize deformation during hot working. SKD1 steel can meet the precision forming requirements of complex molds and has a wide range of applications in fields such as automotive parts and electronic stamping.
    FCS D3 Cold Work Steel | 1.2080 | X210Cr12 | SKD1
    D3 steel has good wear resistance and is suitable for making dies and punches with low impact load and high wear resistance, cold shear knives, drill sleeves, gauges, wire drawing dies, etc.
    FCS 9CrWMn Tool Steel
    9CrWMn steel is a cold work die steel with high hardness, excellent wear resistance, and small quenching deformation, known as "micro deformation steel". 9CrWMn steel is particularly suitable for manufacturing high-precision molds with small cross-sections and complex shapes, such as cold stamping dies, gauges, etc.
    1.2842 Tool Steel
    1.2842 steel is suitable for manufacturing precision measuring tools, templates, small stamping/cold pressing/carving/cutting molds, and machine tool screws and other structural components. 1.2842 steel is also commonly used to manufacture cold stamping dies and tools with large cross-sections, complex shapes, and heavy working conditions, such as stamping dies, trimming dies, grinding dies, steel plate deep drawing dies, circular saws, standard tools and gauges, rolling dies, etc.
    A2 Tool Steel
    A2 Tool Steel is a versatile, air-hardening tool steel that is characterized by good toughness and excellent dimensional stability in heat treatment.
    NC6 Tool Steel
    NC6 steel is a tool steel with medium to high hardness, good processing performance, and excellent wear resistance, mainly used for manufacturing cutting tools, drill bits, stamping molds, etc. NC6 steel has small bending and dimensional changes during quenching, but low toughness and poor tempering resistance.
    X153CrMoV12 Steel
    X153CrMoV12 steel is suitable for making all kinds of cold stamping dies with large cross-section and complex shape, as well as cold cutting scissors and thread taking plates; Cold extrusion forming, trimming die, etc
    X210CrW12 Steel
    X210CrW12 steel is a high carbon, high chromium tungsten alloy tool steel, belonging to cold work die steel. X210CrW12 steel is renowned for its excellent wear resistance, high hardness, and good dimensional stability, making it particularly suitable for manufacturing high-precision, high wear resistant cold work molds and tools.
    FCS 1.2358 tool steel
    1.2358 mold steel has excellent wear resistance and good processing performance, and is widely used in industrial fields such as automotive parts stamping molds, injection mold inserts, precision shear blades, and hot forging molds below 600 ℃ (requiring coating). 1.2358 steel is particularly suitable for high-precision and high load mold manufacturing requirements.

    Products

    Featured products

    • X210Cr12 Steel
      X210Cr12 Steel
      X210Cr12 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
      More
    • Cr12 Tool Steel
      Cr12 Tool Steel
      Cr12 Steel is suitable for the manufacture of cold working dies with complex shape and requiring wear resistance, small deformation and stress, such as silicon steel sheet punching die, thread rolling die and drawing die.
      More
    • K110 Tool Steel
      K110 Tool Steel
      K110 steel is a high carbon, high chromium cold work die steel with extremely high hardness, excellent wear resistance, and good toughness, making it a typical wind hardening tool steel. K110 steel has good dimensional stability during heat treatment and is suitable for high-precision, high load cold work mold manufacturing.
      More
    • A2 Tool Steel | 1.2363 | X100CrMoV5 | SKD12 | BA2 Steel
      A2 Tool Steel | 1.2363 | X100CrMoV5 | SKD12 | BA2 Steel
      A2 steel is a cold work die steel with balanced performance: excellent hardenability, uniform hardness after quenching of large sections; Strong wear resistance, carbide particles delay wear and prolong life; Excellent toughness, impact resistance and minimal cracking under high hardness; Good processability, easy to process in annealed state, quickly recovers high strength after heat treatment, suitable for cold stamping, cutting tools and other scenarios.