Cold Work Tool Steel

    K110 Tool Steel
    K110 steel is a high carbon, high chromium cold work die steel with extremely high hardness, excellent wear resistance, and good toughness, making it a typical wind hardening tool steel. K110 steel has good dimensional stability during heat treatment and is suitable for high-precision, high load cold work mold manufacturing.
    A2 Tool Steel | 1.2363 | X100CrMoV5 | SKD12 | BA2 Steel
    A2 steel is a cold work die steel with balanced performance: excellent hardenability, uniform hardness after quenching of large sections; Strong wear resistance, carbide particles delay wear and prolong life; Excellent toughness, impact resistance and minimal cracking under high hardness; Good processability, easy to process in annealed state, quickly recovers high strength after heat treatment, suitable for cold stamping, cutting tools and other scenarios.
    1.2510 Tool Steel
    1.2510 steel is suitable for making wear-resistant and non deformed cold working dies, jewelry embossing dies, various metal stamping dies and forming tools, mold bushings and cutting tools.
    SKD11 Tool Steel
    SKD11 tool steel is a high wear-resistant cold working die steel, which belongs to air hardened tool steel. It can be used to manufacture cold working die steel with large section, complex shape, large impact force and high wear resistance. SKD11 tool steel is suitable for complex and possibly deformed tool steel, all kinds of cold stamping dies with high wear resistance and long life, cold shear blades and wire rubbing plates; Cold extrusion forming, drawing die, beer stainless steel sheet and blanking die for high hardness materials, etc.
    AISI D6 Tool Steel | 1.2436 | X210CrW12 | SKD2 Cold Work Steel
    D6 tool steel has the characteristics of high hardenability, hardenability, strength and toughness, wear resistance and small quenching volume deformation. D6 tool steel is suitable for cold stamping die, wire drawing die, drawing die, embossing die, wire rolling die, wire rolling plate, cold upsetting die and cold extrusion die.
    X12MΦ Tool Steel
    X12MΦ steel is suitable for stamping dies, cold extrusion dies, wire rollers, wire rings, cold scissors, and precision measuring tools with complex shapes.
    Cr12MoV Tool Steel
    Cr12MoV steel is suitable for blanking die steel, drawing die, thread rolling die, thread rolling plate, and die with complex shape and impact load.
    Cr12W Tool Steel
    The highlight of Cr12W steel as a high-end cold work die steel lies in its excellent wear resistance (62-64HRC) and perfect balance of toughness. Cr12W steel significantly improves its red hardness by adding 1% tungsten element, ensuring stable performance of the die at 300 ℃; The optimized carbide distribution of Cr12W steel gives it three times the service life of ordinary mold steel, making it particularly suitable for precision electronic component stamping and automotive part forming.
    1.2436 Tool Steel
    1.2436 steel is suitable for medium load stamping die, stamping stainless steel, copper, silicon, aluminum, etc.
    1.2601 Tool Steel
    1.2601 is used to manufacture various cold punching dies and tools with large cross-section, complex shape and heavy working conditions, such as punching die, trimming die, edge rolling die, steel plate deep drawing die, circular saw, standard tools and gauges, thread rolling die, etc.

Products

Featured products

  • 1.2363 Steel
    1.2363 Steel
    1.2363 steel has excellent wear resistance and compressive strength, while maintaining good toughness, making it particularly suitable for manufacturing high-precision cold work molds.
    More
  • FCS O1 Tool Steel | 1.2510 | 100MnCrW4 | SKS3
    FCS O1 Tool Steel | 1.2510 | 100MnCrW4 | SKS3
    O1 mold steel is widely used. O1 steel has good processability, good wear resistance, stable O1 heat treatment performance, small dimensional deformation, but weak toughness and corrosion resistance. It is commonly used in blanking die, punching die, punching die, punching die, etc.
    More
  • D3 Tool Steel
    D3 Tool Steel
    D3 steel is suitable for concave and convex dies, inserts, stretching and blanking dies, wire rollers, punches, scissors, etc. with complex shapes.
    More
  • FCS D6 Tool Steel
    FCS D6 Tool Steel
    As a representative of high-end cold work die steel, D6 steel's core highlight lies in achieving excellent balance between wear resistance and crack resistance through high carbon and high chromium alloy design, and significantly improving dimensional stability through deep cryogenic treatment technology; D6 steel exhibits excellent deformation resistance and durability in harsh working conditions such as silicon steel sheet punching and precision processing of high-strength steel plates, while also possessing good corrosion resistance, making it an ideal choice for high-precision and high load mold manufacturing.
    More