Tool Steel

    8418 steel | Tool Steel | Tool Steel Manufacturer
    8418 steel has good properties of resistance to thermal fatigue cracking, thermal shock cracking, thermal wear and plastic deformation. 8418 steel is often used in zinc, magnesium, aluminum and titanium alloy die casting molds, hot extrusion molds, hot forging molds, etc.
    SKD11 Tool Steel
    SKD11 tool steel is a high wear-resistant cold working die steel, which belongs to air hardened tool steel. It can be used to manufacture cold working die steel with large section, complex shape, large impact force and high wear resistance. SKD11 tool steel is suitable for complex and possibly deformed tool steel, all kinds of cold stamping dies with high wear resistance and long life, cold shear blades and wire rubbing plates; Cold extrusion forming, drawing die, beer stainless steel sheet and blanking die for high hardness materials, etc.
    AISI D6 Tool Steel | 1.2436 | X210CrW12 | SKD2 Cold Work Steel
    D6 tool steel has the characteristics of high hardenability, hardenability, strength and toughness, wear resistance and small quenching volume deformation. D6 tool steel is suitable for cold stamping die, wire drawing die, drawing die, embossing die, wire rolling die, wire rolling plate, cold upsetting die and cold extrusion die.
    1.2436 Tool Steel
    1.2436 steel is suitable for medium load stamping die, stamping stainless steel, copper, silicon, aluminum, etc.
    1.2365 Tool Steel | ASTM H10 | 32CrMoV12-28 | SKD7 | BH10
    1.2365 tool steel has high heat resistance, impact and fatigue, and good thermal conductivity. 1.2365 tool steel is suitable for high-pressure working tools, hot die forging press steel, copper, non ferrous metals and pressure casting molds.
    H13 Tool Steel | 1.2344 | X40CrMoV5-1 | SKD61 Hot Work Steel
    H13 hot working die steel. It has excellent machinability and polishing performance, high toughness and plasticity, good high and low temperature wear resistance, high temperature fatigue and heat resistance. H13 tool steel can be used for die forging hammer forging die, aluminum alloy die casting die, hot extrusion die, high-speed precision forging die and forging press die, etc.
    L6 Tool Steel | 1.2713 | 55NiCrMoV7 | SKT4 | BH224/5
    L6 steel is a multi-purpose Oil hardened, heat-resistant and wear-resistant forged steel tool steel with very good toughness. L6 tool steel is suitable for tools, molds and mechanical parts. They need a good combination of hardness and toughness. The relatively high nickel content makes the alloy have greater impact toughness than other ordinary oil hardening grades.
    HD Hot Work Tool Steel
    HD steel is a kind of high toughness, air cooling hardening hot working die steel. HD steel has good high temperature strength and toughness, high temperature hardness, thermal stability and thermal fatigue resistance. HD steel is often used for hot extrusion punch of steel medicine pipe, extrusion bottom die and perforation needle of copper alloy pipe, hot extrusion bearing punch and concave die, valve extrusion low die and so on. The service life is longer than that of H21 steel.
    FCS 1.2316 Tool Steel
    1.2316 is a kind of pre hardened and tempered plastic tool steel. Excellent corrosion resistance, excellent wear resistance and toughness, good thermal fatigue resistance, uniform material hardness and superior polishing performance. 1.2316 tool steel is especially suitable for thermoplastic corrosive plastics, transparent and mirror products and molds.
    FCS 1.2767 Tool Steel
    1.2767 steel has good wear resistance, high toughness, high hardness, high compressive strength, excellent dimensional stability, excellent corrosion resistance, good polishing and pin cutting performance, and easy to achieve mirror effect. Good hardenability, air cooling hardening, good machining performance.

Products

Featured products

  • FCS 420SS Tool Steel
    FCS 420SS Tool Steel
    420SS steel is a martensitic stainless steel known for its excellent hardness and corrosion resistance. After heat treatment, it can achieve high hardness while maintaining a certain degree of toughness, making it very suitable for manufacturing parts that require wear resistance and rust prevention, such as cutting tools, surgical instruments, and precision mechanical components.
    More
  • D2 Tool Steel | 1.2379 | X155CrVMo12-1 | SKD11
    D2 Tool Steel | 1.2379 | X155CrVMo12-1 | SKD11
    As a benchmark for high carbon and high chromium cold work die steel, D2 steel's core highlight lies in the precise ratio of 12% chromium content and 1.5% carbon to form a large number of hard carbides. It maintains an ultra-high hardness of 60-62HRC while also having better wear resistance than ordinary tool steel (5-8 times that of ordinary steel). After appropriate heat treatment, D2 steel can significantly improve its anti cracking performance, especially suitable for high-strength wear scenarios such as precision punching dies and shear cutting tools. D2 steel, known as "semi stainless steel", also forms a passive film on its surface to delay corrosion, becoming a classic choice for balancing performance and cost in the industrial field.
    More
  • 1.2080 Tool Steel
    1.2080 Tool Steel
    1.2080 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
    More
  • FCS 1.2083 Tool Steel
    FCS 1.2083 Tool Steel
    1.2083 steel is suitable for die casting of steel, die and pressure tools and light non-ferrous metal alloys that are easily affected by corrosive plastic and polymer tools and inserts.
    More