1.2365 Tool Steel | ASTM H10 | 32CrMoV12-28 | SKD7 | BH10

1.2365 tool steel has high heat resistance, impact and fatigue, and good thermal conductivity. 1.2365 tool steel is suitable for high-pressure working tools, hot die forging press steel, copper, non ferrous metals and pressure casting molds.
  • fucheng steel
  • China
  • 1 Month
  • 2000 Tons/Month

1.2365 TOOL STEEL

Smelting and Manufacture Method:LF+VD+Forged
Delivery Condition:Annealed
Delivery hardness:≤229 HBS
UT Test Standard: Sep 1921-84 Class3 D/d,E/e

1.2365 TOOL STEEL

H10 Steel

1.2365 STEEL GRADE COMPARISON AND CHEMICAL COMPOSITION COMPARISON

Standard/Steel GradeChemical Composition(%)
CSiMnCrMoV
ASTMH100.35~0.450.80~1.200.25~0.703.00~3.752.00~3.000.25~0.75
DIN/W-Nr.X32CrMoV3-3/1.23650.28~0.350.10~0.400.15~0.452.70~3.202.60~3.000.40~0.70
JISSKD70.28~0.350.10~0.400.15~0.452.70~3.202.50~3.000.40~0.70


APPLICATION

1.2365 tool steel is suitable for high-pressure working tools, hot die forging press steel, copper, non ferrous metals and pressure casting molds.


1.2365 Steel Characteristics


1.2365 steel is a tool steel with high heat resistance, impact resistance, and fatigue resistance, which has good thermal conductivity, hot tensile strength, resistance to rebound, and high toughness brought about by fine grain size. In addition, it has an additional fine structure without grain boundaries, and hard alloys with high creep strength exhibit stability at higher temperatures, making it insensitive to constant temperature changes. This characteristic enables 1.2365 steel to maintain good mechanical properties under high temperature conditions. At the same time, it is suitable for water cooling, which means that it can effectively cool during use and improve the service life of the tool.


Due to its excellent performance, 1.2365 steel is widely used in fields such as automotive manufacturing, aerospace, mechanical manufacturing, electronics and electronics. For example, in automotive manufacturing, it can be used to manufacture engine parts, brake systems, etc; In the field of aerospace, it can be used to manufacture aircraft engine parts, rocket engine nozzles, etc; In mechanical manufacturing, it can be used to manufacture machine tools, molds, etc; In the field of electronic appliances, it can be used to manufacture electronic components, etc.


However, although 1.2365 steel has many advantages, it also has some limitations. Firstly, due to its high cobalt content, its cost is relatively high, which may increase manufacturing costs. Secondly, although it has good wear and corrosion resistance, its corrosion resistance may decrease in special environments such as strong acids and alkalis. Therefore, in certain special application scenarios, it may be necessary to choose other types of steel. Finally, due to its high hardness, special care is required during heat treatment to prevent the generation of cracks and other heat treatment defects.


During the use of 1.2365 steel, it is also necessary to pay attention to some maintenance and upkeep issues. Firstly, regular cleaning and maintenance should be carried out to prevent rust and other surface contamination. Secondly, during use, severe impact and excessive pressure should be avoided to prevent cracks and other damage. Finally, if any abnormal wear or damage is found, it should be promptly inspected and repaired to prevent further deterioration of the problem.


SKD7 Steel

1.2365 TOOL STEEL

H10 Steel

SKD7 Steel

1.2365 TOOL STEEL


Related Products

40px

80px

80px

80px

Get the latest price? We will reply as soon as possible (within 12 hours)

40px

40px

40px

40px