Hot Work Tool Steel

    8418 steel | Tool Steel | Tool Steel Manufacturer
    8418 steel has good properties of resistance to thermal fatigue cracking, thermal shock cracking, thermal wear and plastic deformation. 8418 steel is often used in zinc, magnesium, aluminum and titanium alloy die casting molds, hot extrusion molds, hot forging molds, etc.
    1.2365 Tool Steel | ASTM H10 | 32CrMoV12-28 | SKD7 | BH10
    1.2365 tool steel has high heat resistance, impact and fatigue, and good thermal conductivity. 1.2365 tool steel is suitable for high-pressure working tools, hot die forging press steel, copper, non ferrous metals and pressure casting molds.
    H13 Tool Steel | 1.2344 | X40CrMoV5-1 | SKD61 Hot Work Steel
    H13 hot working die steel. It has excellent machinability and polishing performance, high toughness and plasticity, good high and low temperature wear resistance, high temperature fatigue and heat resistance. H13 tool steel can be used for die forging hammer forging die, aluminum alloy die casting die, hot extrusion die, high-speed precision forging die and forging press die, etc.
    L6 Tool Steel | 1.2713 | 55NiCrMoV7 | SKT4 | BH224/5
    L6 steel is a multi-purpose Oil hardened, heat-resistant and wear-resistant forged steel tool steel with very good toughness. L6 tool steel is suitable for tools, molds and mechanical parts. They need a good combination of hardness and toughness. The relatively high nickel content makes the alloy have greater impact toughness than other ordinary oil hardening grades.
    5CrNiMo Hot Work Tool Steel
    5CrNiMo tool steel is suitable for manufacturing large and medium-sized hammer forging dies and trimming dies with complex shapes, large impact load and low working temperature.
    1.2367 Tool steel
    The highlight of 1.2367 steel lies in its perfect performance balance: it maintains excellent toughness even at 62HRC ultra-high hardness, and its wear resistance life is more than three times that of ordinary mold steel; 1.2367 steel has excellent dimensional stability after deep cryogenic treatment (0.002mm/100mm), and maintains accuracy even after 2 million stamping cycles; The optimized heat treatment process of 1.2367 steel has increased processing efficiency by 40%, making it the preferred material for precision electronic molds.
    4Cr5MoSiV Mold Steel
    4Cr5MoSiV mold steel has good thermal strength and heat fatigue resistance, and can maintain stable performance under high temperature conditions. 4Cr5MoSiV mold steel is widely used in die-casting molds, injection molds, plastic molds and other fields.
    HD Hot Work Tool Steel
    HD steel is a kind of high toughness, air cooling hardening hot working die steel. HD steel has good high temperature strength and toughness, high temperature hardness, thermal stability and thermal fatigue resistance. HD steel is often used for hot extrusion punch of steel medicine pipe, extrusion bottom die and perforation needle of copper alloy pipe, hot extrusion bearing punch and concave die, valve extrusion low die and so on. The service life is longer than that of H21 steel.
    4X5MΦC Hot Work Tool Steel
    Сталь 4X5MΦC обладает высокой твердостью и ударной вязкостью и подходит для литья под давлением, экструзии, горячего прессования алюминия, меди, магния.
    8407 steel | Tool Steel | Tool Steel factory
    8407 hot working die steel. Steel with high purity and fine structure obtained by special steelmaking technology and strict quality control, It has excellent machinability and polishing performance, high toughness and plasticity, good high and low temperature wear resistance, high temperature fatigue and heat resistance. 8407 tool steel can be used for die forging hammer forging die, aluminum alloy die casting die, hot extrusion die, high-speed precision forging die and forging press die, etc.

Products

Featured products

  • 1.2581 Hot Work Tool Steel
    1.2581 Hot Work Tool Steel
    1.2581 hot work mold steel is a commonly used die-casting mold steel. 1.2581 steel has high strength and hardness, good resistance to cold and hot fatigue, and good hardenability.
    More
  • 1.2343 Tool Steel
    1.2343 Tool Steel
    1.2343 steel is a hot work die steel with high toughness and wear resistance. Its core advantages lie in excellent heat fatigue resistance and high-temperature strength. 1.2343 steel is very suitable for high-temperature working environments such as die-casting and forging.
    More
  • SKD61 Hot Work Tool Steel
    SKD61 Hot Work Tool Steel
    As a Japanese JIS standard hot work die steel, SKD61 steel's core highlights include excellent high-temperature performance, outstanding wear resistance and toughness, good processing performance, corrosion resistance, and wide applicability. SKD61 steel ensures material purity through vacuum degassing and electric slag remelting processes, combined with a heat treatment process of 1020-1050 ℃ quenching+550-680 ℃ triple tempering, which increases mold life by more than 50%.
    More
  • S7 Tool Steel
    S7 Tool Steel
    S7 steel is a kind of air or Oil hardened tool steel with high impact toughness. The combination of strength and high toughness makes it a candidate for various tool applications. S7 tool steel is often used for cold working tools that need to resist high impact and impact loads, such as shear blades, forging dies, clamping dies, chisels and punches.