1.3355 High Speed Steel

1.3355 high speed steel has good ductility and is used for roughing and finishing tools with medium strength parameters. 1.3355 high speed steel can be used to produce turning tools, chisel tools, turning and planer, milling cutter, drill bit, thread tool, saw blade, planer, small circular saw, reamer, tap and screw cutter processed on automatic machinery.
  • fucheng steel
  • China
  • 1 Month
  • 2000 Tons/Month

1.3355 HIGH SPEED STEEL

Smelting and Manufacture Method:LF+VD+Forged
Delivery Condition:Annealed
Delivery hardness:≤300 HBS
UT Test Standard: Sep 1921-84 Class3 D/d,E/e

1.3355 Steel

T1 Tool Steel

1.3355 STEEL GRADE COMPARISON AND CHEMICAL COMPOSITION COMPARISON

Standard/Steel GradeChemical Composition(%)
CSiMnCrVW
DIN/W-Nr.S18-0-1/1.33550.70~0.78≤0.45≤0.403.80~4.501.00~1.2017.50~18.50
ASTMT10.65~0.800.20~0.400.10~0.403.75~4.500.90~1.3017.25~18.75
JISSKH20.73~0.83≤0.45≤0.403.80~4.501.00~1.2017.20~18.70


APPLICATION

1.3355 high speed steel can be used to produce turning tools, chisel tools, turning and planer, milling cutter, drill bit, thread tool, saw blade, planer, small circular saw, reamer, tap and screw cutter processed on automatic machinery.


1.3355 STEEL CHARACTERISTICS


1.3355 steel is a special type of tool steel, also known as high-speed steel. It is an alloy steel composed of multiple elements, with excellent hardness, toughness, and wear resistance, and is therefore widely used in the manufacturing of various cutting tools, molds, and parts.


The hardness of 1.3355 steel is very high. This is due to its special chemical composition and processing technology. This steel contains a large amount of elements such as tungsten, molybdenum, and chromium, which can form hard phases such as carbides and nitrides at high temperatures, thereby improving the hardness of the steel. Generally speaking, the hardness of 1.3355 steel can reach between HRC68-70, which makes it have excellent wear resistance and durability when manufacturing cutting tools.


1.3355 steel also has good toughness and ductility. Despite its high hardness, it still has a certain degree of toughness and can withstand large impact and vibration loads. In addition, the steel also has good ductility, and its physical properties such as hardness and strength can be adjusted through heat treatment to meet the needs of different applications.


1.3355 steel has excellent wear resistance. Due to its high content of hard phases, it can still maintain good performance under high-speed cutting and wear conditions. At the same time, the steel also has a lower friction coefficient and good self-lubricating performance, which can reduce heat and wear during the cutting process. Therefore, it is widely used to manufacture various cutting tools, such as turning tools, milling cutters, drill bits, etc.


1.3355 steel also has good thermal stability and red hardness. This steel can still maintain its physical properties such as hardness and strength at high temperatures, and is not prone to deformation and softening. At the same time, the steel also has good tempering stability, which can maintain its excellent performance even after multiple tempering treatments. These characteristics make 1.3355 steel one of the ideal materials for manufacturing cutting tools.


1.3355 steel also has good processing performance and economy. This steel can be manufactured into various shapes and sizes of tools and parts through various processing techniques such as forging, rolling, and extrusion. Meanwhile, the cost of this steel is relatively low, which can save costs for manufacturers and provide more economical solutions.


In summary, 1.3355 steel, as a special type of tool steel, has excellent characteristics such as hardness, toughness, wear resistance, thermal stability, and economy. It is widely used in the manufacturing of various cutting tools, molds, and parts, making important contributions to the development of the manufacturing industry. With the continuous progress of technology and industrial development, the application prospects of 1.3355 steel will be even broader.


SKH2 Tool Steel

1.3355 Steel

T1 Tool Steel

SKH2 Tool Steel

1.3355 Steel