1.2080 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
X210Cr12 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
Cr12 Steel is suitable for the manufacture of cold working dies with complex shape and requiring wear resistance, small deformation and stress, such as silicon steel sheet punching die, thread rolling die and drawing die.
The highlight of Cr12W steel as a high-end cold work die steel lies in its excellent wear resistance (62-64HRC) and perfect balance of toughness. Cr12W steel significantly improves its red hardness by adding 1% tungsten element, ensuring stable performance of the die at 300 ℃; The optimized carbide distribution of Cr12W steel gives it three times the service life of ordinary mold steel, making it particularly suitable for precision electronic component stamping and automotive part forming.
1.2080 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
X210Cr12 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
Cr12 Steel is suitable for the manufacture of cold working dies with complex shape and requiring wear resistance, small deformation and stress, such as silicon steel sheet punching die, thread rolling die and drawing die.