1.2080 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
X210Cr12 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
Cr12 Steel is suitable for the manufacture of cold working dies with complex shape and requiring wear resistance, small deformation and stress, such as silicon steel sheet punching die, thread rolling die and drawing die.
1.2080 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
X210Cr12 steel has high wear resistance and long service life, and is suitable for various cold stamping dies, cold shear blades, thread take-up plates and other complex and possibly deformed tool dies.
Cr12 Steel is suitable for the manufacture of cold working dies with complex shape and requiring wear resistance, small deformation and stress, such as silicon steel sheet punching die, thread rolling die and drawing die.