1.2083

    FCS 420SS Tool Steel
    420SS steel is a martensitic stainless steel known for its excellent hardness and corrosion resistance. After heat treatment, it can achieve high hardness while maintaining a certain degree of toughness, making it very suitable for manufacturing parts that require wear resistance and rust prevention, such as cutting tools, surgical instruments, and precision mechanical components.
    FCS 1.2083 Tool Steel
    1.2083 steel is suitable for die casting of steel, die and pressure tools and light non-ferrous metal alloys that are easily affected by corrosive plastic and polymer tools and inserts.
    FCS 4Cr13 Plastic Mould Steel
    The biggest advantage of 4Cr13 steel is its high hardness, good wear resistance, and good corrosion resistance. 4Cr13 steel is particularly suitable for manufacturing cutting tools, medical devices, molds, and durable parts that require rust prevention.
    S136 / S136H
    S136 steel is a high-end mirror mold steel with excellent corrosion resistance and polishing performance, with a hardness of 50-54HRC. S136 steel is particularly suitable for precision optical molds and corrosive plastic molding.
    AISI 420SS | DIN 1.2083 | JIS SUS420J2
    1.2083 steel is a high chromium stainless steel with excellent corrosion resistance, high hardness, and wear resistance, as well as good polishing performance. 1.2083 steel is commonly used to manufacture high demand plastic molds and optical components.

    Products

    Featured products

    • FCS 420SS Tool Steel
      FCS 420SS Tool Steel
      420SS steel is a martensitic stainless steel known for its excellent hardness and corrosion resistance. After heat treatment, it can achieve high hardness while maintaining a certain degree of toughness, making it very suitable for manufacturing parts that require wear resistance and rust prevention, such as cutting tools, surgical instruments, and precision mechanical components.
      More
    • FCS 1.2083 Tool Steel
      FCS 1.2083 Tool Steel
      1.2083 steel is suitable for die casting of steel, die and pressure tools and light non-ferrous metal alloys that are easily affected by corrosive plastic and polymer tools and inserts.
      More
    • FCS 4Cr13 Plastic Mould Steel
      FCS 4Cr13 Plastic Mould Steel
      The biggest advantage of 4Cr13 steel is its high hardness, good wear resistance, and good corrosion resistance. 4Cr13 steel is particularly suitable for manufacturing cutting tools, medical devices, molds, and durable parts that require rust prevention.
      More
    • S136 / S136H
      S136 / S136H
      S136 steel is a high-end mirror mold steel with excellent corrosion resistance and polishing performance, with a hardness of 50-54HRC. S136 steel is particularly suitable for precision optical molds and corrosive plastic molding.
      More