    Y4 Hot Work Tool Steel
    Y4 steel has high thermal strength and thermal stability, good toughness, thermal conductivity, process performance and good forging performance. Y4 steel is a heat-resistant die steel for making die-casting die. In the environment of use, it should bear high temperature, high pressure and high impact.