M2 steel is a tungsten molybdenum high-speed steel with good hardness and wear resistance. Mainly used for manufacturing cutting tools for difficult to cut materials.
M2 high-speed steel is suitable for molds that can withstand vibration and impact loads: deep drawing molds, stamping molds, metal cutting blades, cold heading and extrusion tools.