D6 Tool Steel

    AISI D6 Tool Steel | 1.2436 | X210CrW12 | SKD2 Cold Work Steel
    D6 tool steel has the characteristics of high hardenability, hardenability, strength and toughness, wear resistance and small quenching volume deformation. D6 tool steel is suitable for cold stamping die, wire drawing die, drawing die, embossing die, wire rolling die, wire rolling plate, cold upsetting die and cold extrusion die.