95Cr18 steel is a high carbon and high chromium martensitic stainless steel, which has the core advantages of ultra-high hardness, excellent wear resistance, and significant corrosion resistance. 9Cr18 stainless steel can achieve a balance of strength and toughness through precise heat treatment process, and is widely used in fields such as surgical tools, bearings, chemical pumps and valves that require both hardness and corrosion resistance.