8418 steel has good properties of resistance to thermal fatigue cracking, thermal shock cracking, thermal wear and plastic deformation.
8418 steel is often used in zinc, magnesium, aluminum and titanium alloy die casting molds, hot extrusion molds, hot forging molds, etc.