38CrMoV5-3 steel has high high temperature strength, high temperature wear resistance and crack propagation resistance.
38CrMoV5-3 steel is usually used for hot forging dies with high service life requirements, aluminum and zinc die casting dies. Aluminum alloy, copper alloy extrusion die, complex extrusion die.