FCS 1.2714 Hot Work Tool Steel
- fucheng steel
- China
- 1 Month
- 2000 Tons/Month
1.2714 TOOL STEEL
| Brand | FCS |
| Smelting and Manufacture Method: | LF+VD+Forged |
| Delivery Condition: | Annealed |
| Delivery hardness: | ≤241 HBS |
| UT Test Standard: | Sep 1921-84 Class3 D/d,E/e |


1.2714 STEEL GRADE COMPARISON AND CHEMICAL COMPOSITION COMPARISON
| Standard/Steel Grade | Chemical Composition(%) | |||||||
| C | Si | Mn | Cr | Mo | V | Ni | ||
| DIN/W-Nr. | 56NiCrMoV7/1.2714 | 0.50~0.60 | 0.10~0.40 | 0.65~0.95 | 1.00~1.20 | 0.45~0.55 | 0.07~0.12 | 1.50~1.80 |
| ASTM | 6F3 | 0.55 | 0.85 | 0.60 | 1.00 | 0.75 | 0.10 | 1.00 |
| GB | 5CrNiMoV | 0.50~0.60 | ≤0.35 | 0.50~0.80 | 0.80~1.10 | 0.35~0.50 | 0.10~0.30 | 1.40~1.80 |
APPLICATION
1.2714 steel is mainly used in three scenarios: first, hot working molds, such as large forging dies, extruder plungers, hot cutting blades, etc., which can withstand high temperature, high pressure, and frequent thermal cycles; The second is plastic molding molds, especially suitable for large thermoplastic processing molds and injection molds, which can meet the requirements of stability, wear resistance, and deformation prevention; The third is high-strength mechanical components, including shafts, retaining rings, gears, axles, etc., which can cope with high impact and wear conditions.
1.2714 Steel Characteristics
1.2714 steel can maintain stable mechanical properties in sustained high temperature environments in terms of high-temperature strength. This characteristic makes it particularly suitable for high-temperature applications such as die-casting molds.
The outstanding advantage of 1.2714 steel is its resistance to thermal fatigue, as its microstructure can effectively resist thermal stress caused by drastic temperature changes. This feature significantly extends the service life of the mold under rapid cooling and heating conditions.
The corrosion resistance of 1.2714 steel is attributed to its special alloy composition design, which enables the formation of a dense protective layer on the surface of the mold. This characteristic is particularly important in corrosive environments such as aluminum alloy die-casting.
In terms of toughness performance, 1.2714 steel has excellent impact resistance while maintaining high hardness. This balance enables it to withstand mechanical impact loads during the production process.
In terms of processing performance, 1.2714 steel exhibits good machinability in the annealed state. This feature reduces the processing difficulty and cost in the mold manufacturing process.
1.2714 steel has minimal deformation during heat treatment, making it particularly suitable for precision mold manufacturing. This feature ensures the dimensional accuracy and reusability of the mold.
In terms of anti softening ability, 1.2714 steel performs well and can maintain working hardness for a long time. This feature is crucial for extending the service life of molds.