4Cr5MoSiV1 Steel

4Cr5MoSiV1 steel is mainly used for manufacturing hot extrusion molds, die-casting molds, hot forging molds, etc. 4Cr5MoSiV1 steel is widely used in industries such as automotive, machinery, and electronics.
  • Fucheng steel
  • China
  • 1 Month
  • 2000 Tons/Month

4Cr5MoSiV1 TOOL STEEL

Smelting and Manufacture Method:LF+VD+ESR+Forged
Delivery Condition:Annealed
Delivery hardness:≤235 HBS
UT Test Standard: Sep 1921-84 Class3 D/d,E/e

4Cr5MoSiV1 Steel

4Cr5MoSiV1 Tool Steel

4Cr5MoSiV1 STEEL GRADE COMPARISON AND CHEMICAL COMPOSITION COMPARISON

Standard/Steel GradeChemical Composition(%)
CSiMnCrMoV
GB
4Cr5MoSiV1
0.32~0.42
0.80~1.20
0.20~0.50
4.75~5.50
1.10~1.75
0.80~1.20
DIN/W-Nr.X40CrMoV5-1/1.23440.35~0.420.90~1.200.30~0.504.80~5.501.20~1.500.90~1.15
ASTMH130.32~0.450.80~1.200.20~0.504.75~5.501.10~1.750.80~1.20
JISSKD610.35~0.420.80~1.200.25~0.504.80~5.501.00~1.500.80~1.15


APPLICATION

4Cr5MoSiV1 steel is a high-performance hot work die steel, mainly used in die-casting molds, hot forging molds, hot extrusion molds, plastic injection molds, and high-temperature tool manufacturing.

In the field of die casting, 4Cr5MoSiV1 steel is particularly suitable for high-pressure casting of non-ferrous metals such as aluminum alloys and magnesium alloys. It can withstand repeated erosion from high-temperature metal liquids at 700 ℃, significantly extending the life of molds.

In terms of hot forging and hot extrusion, 4Cr5MoSiV1 steel exhibits excellent high temperature resistance, which can maintain stability in an instantaneous high temperature of 1200 ℃ and a continuous working environment of 600 ℃. It is suitable for the forming and processing of automotive parts, copper pipes, aluminum profiles and other products.

After appropriate heat treatment, 4Cr5MoSiV1 steel is widely used in plastic mold manufacturing, especially for injection molding of engineering plastics, as well as the production of high-temperature cutting tools such as continuous casting billet guide wheels and hot shear blades, demonstrating excellent wear resistance, thermal fatigue resistance, and red hardness.


4Cr5MoSiV1 Steel Characteristics


4Cr5MoSiV1 steel can maintain high strength at high temperatures, is not easily softened or deformed, and is suitable for working in high-temperature environments, such as in hot work molds. It can withstand repeated heating and cooling without being easily damaged.
 
4Cr5MoSiV1 steel has good toughness and can withstand a certain degree of impact and vibration, making it less prone to sudden fracture during use.
 
4Cr5MoSiV1 steel has high hardness and a wear-resistant surface, which can maintain a good state for a long time when rubbed or in contact with other objects.
 
4CrMoSiV1 steel can achieve high hardness and strength inside the steel through heat treatment such as quenching, not just on the surface.
 
When 4Cr5MoSiV1 steel works for a long time at high temperature, its performance changes relatively little and it can maintain a relatively stable working state.


4Cr5MoSiV14Cr5MoSiV1 Steel4Cr5MoSiV1 Tool Steel4Cr5MoSiV14Cr5MoSiV1 Steel

40px

80px

80px

80px

Get the latest price? We will reply as soon as possible (within 12 hours)

40px

40px

40px

40px