On March 11, 2025, Hubei Fucheng Special Materials Co., Ltd. showcased its high-end mold steel series at the 27th Korea International Mold Fair (INTERMOLD KOREA 2025). As a leading enterprise in China's high-end mold steel sector, the company's specialty alloy materials and innovative technologies became focal points at the exhibition.
Technological breakthrough
High-performance materials: Special alloy mold steels such as SKD11/H13/1.2379/1.2344, which significantly extend service life compared to traditional materials
Customized Solutions: Support for size customization, precise composition adjustment, and heat treatment process optimization to meet diverse needs
Green Manufacturing: Utilizing vacuum smelting technology, the carbon footprint is reduced by 25% during the production process
The Grand Exhibition
The technical team hosted over 200 professional visitors, including those from South Korea, Japan, Southeast Asia, and other regions
Clients from multiple countries requested on-site material inspection reports and samples, delving into potential collaboration opportunities

Future Directions
Hubei Fucheng stated that it will continue to focus on the high-end mold steel niche, increase R&D investment, and drive innovation and industrial upgrading in the application of special materials in the Asian market.