1.2080 mold steel has attracted much attention in the field of mold manufacturing. 1.2080 is a high carbon and high chromium cold working die steel containing molybdenum and vanadium, with multiple excellent characteristics.

1.2080 mold steel has high wear resistance, high compressive strength, high hardness after quenching, and excellent hardenability. After vacuum degassing and refining, its internal quality is extremely clean, and its good machinability and hardenability enable it to harden by air cooling without worrying about quenching cracks. In addition, the heat treatment deformation is very small, and the quenching deviation is extremely small, making it particularly suitable for mold making with precision requirements.

The wear resistance of 1.2080 mold steel is extremely excellent, suitable for various cold work applications. For example, it performs excellently in punching and forming, and can be used in processes such as bending, forming, deep drawing, edge rolling, compression forming and rotation, extrusion forming, etc; It is also commonly used in the manufacturing of stamping dies, cold extrusion dies, cold extrusion punches, forming rolls for pipes and profiles, flat rolls, etc; It is also widely used in the forming molds of ceramics, bricks, ceramic tiles, grinding wheels, tablets, plastics, as well as thread rolling molds, cold forging molds, forging hammers, molds, gauges, measuring tools, guide rails, shaft sleeves, sleeves, embossing molds, sandblasting nozzles, and other aspects.

With the continuous improvement of mold quality requirements in various industries, the market demand for 1.2080 mold steel continues to grow due to its excellent performance. In the future, it is expected that 1.2080 mold steel will continue to play an important role in the field of mold manufacturing and continuously promote the progress and innovation of industry technology.