        Aluminum Alloy Profile Extrusion Die and Extrusion Production Process
2023-11-04 15:10
 FCS Tool Steel Manufacturer
 
Aluminum extrusion is the aluminum alloy into the extrusion cylinder and apply a certain amount of pressure, so that it flows from a specific die hole, so as to obtain the required cross-section shape and size of a processing method, this extrusion processing method is low-cost, high efficiency, easy to operate, and occupies a considerable proportion of the modern industrial production system, so that aluminum extrusion has become an important basic material in the national economy.
 
 Mold Processing Flow Chart-Flat Mold (Structural Profile without Closed Cavity)
Turning → Scribing → Milling → Drilling → Grinding → Quenching → Tempering → Grinding plane → Fine milling guide groove → Wire cutting → EDM → Polishing → Clamping → Acceptance → Test mold → Nitriding → Warehousing
Combination molds (structural profiles with closed cavities)
 
 Mold Pad
Turning → Scribing → Milling → Drilling → Grinding → Hardening → Tempering → Grinding plane → Acceptance → Warehousing

Die Sleeve
Turning → Scribing → Milling → Drilling → Grinding → Hardening → Tempering → Grinding plane → Fine turning → Acceptance → Warehousing
Heat treatment: Through different quenching and aging regimes, aluminum profiles are given the mechanical properties they deserve.
- In summary, through the above aluminum alloy profile extrusion die and extrusion production process details, let us more thoroughly understand the die production process and ingot casting, extrusion, heat treatment and surface treatment, these processes can achieve the desired results to meet the needs of customers. 
 
  
Our advantage
 
   Global service
Our factory covers an area of 40,000 square meters, with a tool steel output of 2,000 tons/month and 25,000 tons/year.
 
   process production line
We have advanced smelting, refining, vacuum debonding Gas, forging, annealing, machining the whole process production line. ASTM/EN/DIN /JIS standard tool steel can be customized.
 
   24-hour service